Hardness and high heat resistance combined with high electrical and thermal conductivity. The rate of Be is lower than Korbak HC1
| DIN | ASTM | RWMA |
|---|---|---|
| w.nr. -2.1285 | -C 17500 | Class III |
| Hardness | 220-270 HB |
| Yield Strength | 650-840 Mpa |
| Tensile Strength | 680-900 Mpa |
| Electrical Conductivity | %48 I.A.C.S. |
| Gravity | 8,8 gr/cm³ |
| Chemical Composition | Co:1,0 – Ni:1,0- Be:0,5 Other:0,2 Cu: Rest |